Jointing · Socket fusion and electrofusion
Fused joints. No bead in the bore.
Every Anjney line is joined by heat, never by glue or thread. Socket fusion from 20 to 160 mm, electrofusion from 160 to 630 mm. The joint becomes the same material as the pipe.
20 to 160 mm · all three lines
Socket fusion
- Cut and markCut the pipe square, chamfer the edge and mark the insertion depth.
- HeatPush pipe and fitting onto the heated tool, around 260 °C, for the set heating time.
- JoinPull both off and push the pipe into the fitting to the mark, without twisting.
- Hold and coolHold for a few seconds and let it cool. Pipe and fitting are now one material.
160 to 630 mm · all three lines
Electrofusion
- Cut and cleanCut the pipe square and clean the ends.
- ScrapeScrape the oxidised skin from the fusion zone so fresh polymer meets the coil.
- Insert and clampPush both pipes into the coupler to the marks and clamp them.
- ConnectConnect the electrofusion machine. It reads the fitting’s barcode.
- FuseThe machine runs the fusion cycle: the moulded-in coil melts pipe and fitting together.
- CoolFusion indicators rise. Leave to cool before pressure testing. No bead in the bore.
Why not butt fusion
Butt fusion joins two pipe ends face to face and leaves a bead ring inside every joint. Pick a duty to see what that ring does.
Compressed air and gas store energy. When a butt weld has a flaw (low heat soak, wrong pressure, misaligned ends), the notch where the bead meets the bore is where stress gathers under pressure cycling. A gas line does not weep like a water line: a crack can open suddenly.
The internal bead is a ring across the bore at every joint. In effluent and acid or alkali lines, solids and crystals settle behind it. The deposit holds chemicals against the fusion plane, the weakest section of a butt joint, and the joint starts to seep.
Every bead ring narrows the bore and makes the flow swirl behind it. On a network with a hundred joints that is a hundred local losses, permanently. Socket fusion and electrofusion put the extra material outside the pipe, in the fitting, so the bore stays full at every joint.
Illustration of how a flawed or ageing butt weld fails. A correctly made butt weld can pass its pressure test; the bead in the bore is there on every joint either way.
Side by side
| Socket fusion and electrofusion | Butt fusion | |
|---|---|---|
| Bead in the bore | None across the bore. Full flow at every joint. | A melt bead inside every joint narrows the bore and adds pressure drop. |
| Fused area | The whole socket length is fused. | Only the wall-thickness face is fused. |
| Alignment | The socket or coupler aligns the pipe. | Needs facing and precise clamping of both ends. |
| Equipment and space | Hand-held heating tool or a compact control box. Works in tight plant rooms. | A hydraulic machine with clearance all round the pipe. |
| Consistency | Depth marks, and a machine-controlled cycle on electrofusion. | Heat soak, pressure and changeover depend on the welder. |
| Repairs and tie-ins | An electrofusion coupler slides over an installed line. | Pipe ends must move towards each other; hard on fixed lines. |
| Small and thin-wall pipe | Works from 20 mm. | Not practical on small, thin-wall pipe. |
Jointing questions
What jointing method does Anjney use?
Socket fusion from 20 to 160 mm and electrofusion from 160 to 630 mm, on PPCH, PPRCT and PPH. Anjney does not use butt fusion.
Is electrofusion better than butt fusion?
For plant piping, yes in most cases: no bead in the bore, a machine-controlled cycle, a compact machine that works in tight spaces, and couplers that slide over installed pipe for repairs.
Does socket fusion need glue?
No. Heat alone fuses pipe and fitting into one homogeneous material. There is no solvent cement and no cure time.
What temperature is used for socket fusion of PP pipe?
The heating tool runs at around 260 °C. Heating time depends on pipe size; Anjney provides the chart with every tool.
How long before an electrofusion joint can be pressure tested?
After the cooling time printed on the fitting has passed. The fusion indicators show that the cycle was completed.
Enquiry
Send us your line schedule
Tell us the service, pipe sizes and approximate run lengths. Our technical sales team sizes the network and returns a bill of material, with an installed-cost comparison against your current specification.
- Sales+91 93747 89875
- Office+91 79 4800 6581
- Emailmarketing@anjney.com
- Exportexport@anjney.com
- WhatsAppMessage us on WhatsApp