PPCH FR Pneumatic Piping comparison
PPCH vs metal pipe for compressed air
Galvanised iron, mild steel and stainless steel have been the default for compressed air. They corrode, scale and leak at threads, and the compressor pays for all three every hour the plant runs.
Side by side
Figures from the Anjney PPCH catalogue and technical notes. For design work, confirm against the current data sheet.
| Parameter | PPCH FR Pneumatic Piping | Metal pipe (GI, MS, CI, SS) |
|---|---|---|
| Surface roughness, Ra | 0.1–0.3 µm | 1.0–1.7 µm |
| Hazen–Williams C | 145–150 | 130–135 |
| Jointing | Socket fusion and electrofusion; electrically heated, no open flame | Threaded or welded; hot-work permit and fire watch |
| Joint integrity | Homogeneous fused joint, no leak path to age | Threads relax with vibration and temperature swings |
| Wall conductivity | 0.135 Btu/hr·ft·°F | 43.66 Btu/hr·ft·°F (steel) |
| Internal surface | Non-corroding, non-scaling | Corrodes and scales; rust fines carried to tools |
| Adding a drop | One fusion joint | Cut, weld or re-thread, permit, re-test |
| Maintenance | Nil | Recurring |
What it means on your plant
Less pressure drop
A smooth, non-scaling bore and no thread restrictions keep pressure drop low for the life of the line.
Drier air
With wall conductivity two orders of magnitude lower than steel, air stays above its dew point longer and less condensate forms.
Cleaner air
No rust or oxide fines reach valves, cylinders and air tools.
Other comparisons
Enquiry
Send us your line schedule
Tell us the service, pipe sizes and approximate run lengths. Our technical sales team sizes the network and returns a bill of material, with an installed-cost comparison against your current specification.